General Information
- Compact hardcoating unit
- Based on PLATIT LARC® technology (LAteral Rotating Cathodes)
- Coating on tool steels (TS) above 200°C, high speed steels (HSS) 350 - 500°C and on tungsten carbide (WC) between 350 - 700°C
- With Virtual and Tube shutter®
- Loading Capacities
Hard Coatings
- Standard: TiN, TiAlN, AlTiN, nACo®
- Optional: TiCN-MP, TiAlCN, GRADVIC®, ZrN, CrN, CROMVIC®, CROMVIC2® , CrTiN, AlCrN, AlTiCrN, Fi-Vic®, Fi-TIVic®, nACVIc, Ti2N, CROMTIVIC®, CROMTIVIC2®, nACRo®
- Monolayers, Multilayers, nanogradients, nanolayers, nanocomposities, DLC and their combinations
Cycle Times
At continuous operation for coating carbide tools:
- Round shank tools: Ø10 x 70 mm, 162 pcs: 3.25 h
- Inserts: o 20 x 6 mm, 864 pcs: 3.25 h
- Hobs: Ø80 x 180 mm, 6 pcs: 4.8
|

|